Properties | As-sprayed | Heat-treated |
---|---|---|
Tensile Strength | 86 MPa | 71 MPa |
Ductility | 12 % | 38 % |
Hardness | 31 HV (0.1) | 24 HV (0.1) |
Properties | As-sprayed | Heat-treated |
---|---|---|
Tensile Strength | 86 MPa | 71 MPa |
Ductility | 12 % | 38 % |
Hardness | 31 HV (0.1) | 24 HV (0.1) |